The energy absorption process of silicon carbide bulletproof ceramics can be roughly divided into three stages

(1)Initial impact stage: the bullet hits the ceramic surface, blunts the bullet, and absorbs energy in the process of crushing the ceramic surface to form small and hard fragment areas;
(2)Erosion stage: The blunted bullet continues to erode the fragment area, forming a continuous layer of ceramic fragments
(3)Deformation, crack and fracture stage: Finally, tensile stress is generated in the ceramic to break the ceramic, and then the back plate is deformed. The remaining energy is absorbed by the deformation of the back plate. When the bullet hits the ceramic, both the bullet and the ceramic are destroyed.